Significantly higher tensile strength, flexural modulus and HDT, lower water absorption and mould shrinkage and higher surface hardness, elongation at break and volume resistance compared with urea ...
Higher maximum operating temperature, better dielectric constant, tracking resistance and dimensional stability compared with cellulose filled urea formaldehyde. Lower HDT, tensile strength and ...